9. Examples for Polymerization Time:
Polymerization times for Vita VM LC:
In order to achieve hardening appropriate for the material involved, the object to be polymerized
on the 40 mm special rings on the slide has to be placed in the center of the turntable within the
light cone of the halogen lamp. Make sure combined dentures with a plaster model get polyme-
rized from all sides and do not exceed the turntable's inner radius of 6 cm.
Polymeri­
PRE OPAQUE
zation
OPAQUE
PASTE
OPAQUE
powder
3 minutes
5 minutes
Once a layer thickness of 2 mm has been obtained, a final polymerization has to be carried
out.
10
Interimpoly­
Final poly­
merization
merization
up to max.
and pontic of
1,5 mm
max. 2 mm
(fixing)
5 minutes
10 minutes
Note
Main energy source is the halo-
gen lamp in the device, it must
not be switched off.
Re-expose shade areas!
Lamps:
8 x Osram Dulux S 9W/71
1 x Halogen Osram
HLX 15V / 150W