• DELAY
This is a pointing mode similar to SPOT, but with a combination of pointing and stopping time defined as long as the trigger is held in.
Settings
Designation
Wire speed
Voltage
Point
Duration between 2
spots
Self
Pre-gas
Post gaz
Thickness
Arc length
Current
Access to some welding parameters depends on the selected display mode: Settings/User Level: Easy, Expert, Advanced.
MIG/MAG WELDING CYCLES
Standard 2T process:
T hotstart
Dstart
Soft-start
When the trigger is pulled, the Pre-gas starts. When the wire comes into contact with the metal, a pulse ignites the arc and the welding cycle starts.
When the trigger is released, the feeding stops and a current pulse cuts the wire properly followed by the Post gas. While the Post gas is still going,
pulling the trigger allows to quickly restart the weld (manual chain point) without going through the HotStart phase. A HotStart and/or Crater filler
can be added to the cycle.
NEOPULSE 320 C
Adjustable
settings
1 - 22m/min
Quantity of filler metal deposited and indirectly the welding intensity.
10 - Umax
Adjusts the welding power
0.1 - 10 secs.
Defined duration.
Time between the end of a spot (excluding Post gas) and the start of a new spot (including
0.1 - 10 secs.
Pre-Gas).
Smoothes more or less the welding current. To be adjusted according to the welding
-4 > +4
position.
0 - 25 secs.
Torch purge time and to protect the area with gas before ignition
Duration for which gas is released after the arc has stopped. It protects the weld pool and
0 - 25 secs.
the electrode against oxidisation when the metal is cooling down.
The synergy allows for fully automatic settings. The thickness action automatically
0.1 - 5.5 mm
sets the tension and the appropriate yarn speed.
Used to adjust the distance between the end of the wire and the weld (voltage
-6 > +6
adjustment).
The welding current is adjusted according to the type of wire used and the mate-
10 - Imax
rial to be welded.
Description & advice
I
T crater Filler
EN
I blackout
Gas post-Flow
T burn-back
I crater Filler
41

Publicidad

Tabla de contenido
loading

Tabla de contenido