Arc length
Self
Pre-gas
Approach speed
Soft Start
Hot Start
Uplsope
Cold current/Back-
ground current
Pulse frequency
Duty cycle ratio
Downslope
Crater filler
Post gaz
Access to some welding parameters depends on the selected display mode: Settings/User Level: Easy, Expert, Advanced.
TACK WELDING (
Manual or
• SPOT
This welding mode allows the parts to be pre-assembled before welding. Spot welding can be done manually using the trigger or timed at a predefi-
ned pace. This spot welding timer is useful for better reproducibility and when making non-oxidized welds (accessible in the advanced menu).
Settings
Designation
Wire speed
Voltage
Self
Point
Pre-gas
Post gaz
Thickness
Arc length
Current
Access to some welding parameters depends on the selected display mode: Settings/User Level: Easy, Expert, Advanced.
40
PULSEMIG 320 C
Used to adjust the distance between the end of the wire and the weld (voltage adjust-
-6 > +6
ment).
Smoothes more or less the welding current. To be adjusted according to the welding
-4 > +4
position.
0 - 25 secs.
Torch purge time and to protect the area with gas before ignition
Progressive wire speed. Before the arcing, the wire arrives slowly to create the first
50 - 200 %
contact without causing a jolt.
Progressive current rise. In order to avoid abrupt starts or jolts, the current is controlled
0 - 2 secs.
between the first contact and the welding.
The Hot Start is an overcurrent during generated during the arcing phase to prevent
50 - 200 %
the wire from sticking. It is adjustable in intensity (% of welding current) and time
0 - 5 secs.
(seconds).
0 - 2 secs.
Up slope current.
50 - 100 %
Second welding current known as «cold» welding current
0.1 - 2 Hz
Pulse frequency
20 - 80 %
In pulsed mode, sets the hot current time in relation to the cold current time.
0 - 2 secs.
Down slope current.
This current treshold when stopped is a phase after the current downslope.
50 - 100 %
It is adjustable in intensity (% of welding current) and time (seconds).
Duration for which gas is released after the arc has stopped. It protects the weld pool
0 - 25 secs.
and the electrode against oxidisation when the metal is cooling down.
Standard (Dynamic STD))
Adjustable
settings
1 - 22m/min
Quantity of filler metal deposited and indirectly the welding intensity.
10 - Umax
Sets the welding power.
Smoothes more or less the welding current. To be adjusted according to the welding
-4 > +4
position.
0.1 - 10 secs.
Defined duration.
0 - 25 secs.
Torch purge time and to protect the area with gas before ignition
Duration for which gas is released after the arc has stopped. It protects the weld pool
0 - 25 secs.
and the electrode against oxidisation when the metal is cooling down.
The synergy allows for fully automatic settings. The thickness action automatically
0.1 - 5.5 mm
sets the tension and the appropriate yarn speed.
Used to adjust the distance between the end of the wire and the weld (voltage
-6 > +6
adjustment).
The welding current is adjusted according to the type of wire used and the mate-
10 - Imax
rial to be welded.