Problem
Cause
The welding pearl is
• The welding current is too low.
very narrow and bulky.
• The welding current is too fast.
Thee welding pearl is
• The welding current is too high.
too wide.
• The welding speed is too slow.
• The arc is too long.
The weld has low
• The welding speed is too slow.
penetration.
• The arc is too long.
The weld has too
• The welding current is too high.
much penetration.
• The welding speed is too slow.
• The arc is too long.
If after all the recommended actions have been carried out the problems persist,

Symbology

DC symbol
Electric arc manual welding with coated electrode
Inert metal – active gas welding, including the use of flux core
Input circuit, single-phase alternating current and rated frequency symbol
~
1
60 Hz
Work cycle symbol (service factor)
X
Nominal welding current symbol
I
2
Conventional load voltage symbol
U
2
Rated open circuit voltage
U
... V
0
Rated power voltage
U
... V
1
Maximum rated power
I
... A
1 max
Maximum effective power
I
... A
1 eff
Protection degree (solid objects and water submersion)
IP
Converter - transformer - single-phase static frequency rectifier
1
˜
f
f
1
2
AC symbol
Electric-arc manual welding with coated electrodes
SMAW
Gas shielded arc welding system
TIG
Metal inert gas welding
MIG
Tungsten inert gas welding
contact a
Solution
• Increase the micro wire current and speed .
• Displace the torch slower and / or make circular or
zigzag movements with the nozzle.
• Diminish the micro wire current and speed.
• Displace the torch faster and / or use less circular
or zigzag movements with the nozzle.
• Correct the distance between the nozzle and the
work piece (from 0.31" to 0.39").
• Increase the micro wire current and speed.
• Correct the distance between the nozzle and the
work piece (from 0.31" to 0.39").
• Diminish the micro wire current and speed.
• Displace the torch faster. No dot make circular or
zigzag movements with the nozzle.
• Correct the distance between the nozzle and the
work piece (from 0.31" to 0.39").