JobMaster TIG
Using the „Mode" button select one of the following parameters:
Set the parameters using the Up/Down function
Cap-shaping - precondition:
-
Intermediate lowering - precondition:
-
-
NOTE!
Frequent bending of the flexible burner can cause permanent damage (no gua-
rantee).
22
Set up welding torch
Adjust current (may also be adjusted during the welding process):
-
0 = min. welding current
-
9 = max. welding current
Touch the workpiece with the tungsten electrode:
-
gas flow starts
-
Arc ignites
End welding using the „TCS - TIG-ComfortStop" feature (see TP 1500 opera-
ting instructions)
TIG-AC welding process
Standard 4-step mode
Set-up parameter SFS must be set to "OFF" (factory setting)